Superalloy Forgings

Superalloy forgings are formulated using nickel, cobalt, or iron as a base, supplemented with significant quantities of alloying elements. These alloying elements are strategically chosen to deliver exceptional strength, toughness, and durability, particularly in environments characterized by high temperatures.
Nickel Based Alloys
We produce forged products for components that must withstand harsh conditions. These alloys have high heat and corrosion resistance, making them ideal for use in jet engines, chemical plants, and many other applications where temperatures are extremely high.
Our Hastelloy and Inconel forging capabilities include forging round and flat bars, rings, blocks and custom shapes.

Material grades

GradeUNS NumberDINWerkstoff Nr
Alloy 718N07718NiCr19Fe19Nb5Mo32.4668
Alloy 718 Plus
WaspaloyN07001NiCr20Co13Mo4Ti3Al2.4654
Alloy 909N19909X4NiCo38Nb
Alloy 907N19907X4NiCo38Nb
Alloy 625N06625NiCr22Mo9Nb2.4856
Alloy 600N06600NiCr15Fe82.4816
Alloy 617N06617NiCr23Co12Mo2.4663
Alloy XN06002NiCr22Fe18Mo2.4665
Alloy H230N06230NiCo29Cr28Si2.4880
Alloy 188R30188CoCr22NiW2.4683
Alloy H242N10242
Alloy HR120N08120NiFe33Cr25Co2.4854
Nimonic 80N07080NiCr20TiAl2.4952
Alloy 825N08825NiCr 21 Mo2.4858
Alloy 800 HN08800 / N08810X8 NiCrAlTi 32-211.4876 / 1.4958
Alloy C276N10276NiMo 16 Cr 15 W2.4819
Monel 400N04400NiCu 30 Fe2.4360
Alloy C263N07263NiCo20Cr20Mo6Ti2Al2.4650
Alloy 286S66286X5 NiCrTi 26-15 1.4980
Rene 41N07041NiCr19Co11MoTi2.4973
Thermo Span

Forged metal products from Qilu

Forged Steel Blocks

Forged Steel Blocks

Our forged steel blocks are crafted from top-tier materials, carefully processed through the steel forging method. As a result, they exhibit outstanding wear resistance and ductility, rendering them superior to castings. This is particularly advantageous in applications demanding heightened strength and extended service life.
Why purchase Forged Steel Blocks from qilu
Our process ensures a minimum reduction area ratio of 3 to 1, ensuring the highest block integrity.
In contrast to castings or flat-rolled products, the forging process imparts directional grain flow and a refined metallurgical microstructure, enhancing mechanical properties such as impact and tensile strength.
At Qilu, we are your comprehensive forging solution. We go beyond forging, offering value-added services like heat treatment, machining, and rigorous testing to provide you with the ultimate solution.

Disc Forgings

Our distinctive capabilities result in disc forgings that are not only flatter and more substantial but also possess outstanding mechanical attributes. These attributes make them the perfect choice for demanding applications such as mills, gear manufacturing, heat exchangers, mining equipment, and heavy machinery. Our disc forgings are crafted using cutting-edge equipment and premium materials, guaranteeing robust, precise, and dependable products.
Why purchase Disc Forgings from qilu
The forging process imparts directional grain flow, enhancing the mechanical performance of our discs.
We offer disc forgings with dimensions of up to 106 inches in outside diameter and a weight of up to 55,000 lbs, catering to both individual custom orders and high-production runs.
At Qilu, we excel in rapid turnaround times, product innovation, and professional consultation to lower costs, reduce machining time, and elevate the overall performance of parts and products.

Steel Flange

Our Steel Flanges are meticulously forged to provide exceptional strength, precision, and resilience. With a wide range of sizes and customization options, we offer flanges that meet the unique demands of various industries, including oil & gas, petrochemical, power generation, and construction. Whether it’s a standard specification or a bespoke solution, our steel flanges ensure the highest level of performance and safety in critical applications.
Why purchase Steel Flange from qilu
We provide flexibility in size and weight for our steel flange, and we can tailor the chemistry to meet the specific needs of our customers.
Our manufacturing process includes rigorous control to ensure the absence of non-metallic inclusions.
At Qilu, we are committed to upholding high manufacturing standards, delivering clean steel compositions, and maintaining impeccable surface quality in every product.

Hollow Tube Forgings

Our hollow tube forgings an inside diameter that is forged directly into the parts, rather than being bored from solid bars. This unique approach significantly reduces production time and enhances overall efficiency. By forging these components as a single unit, we ensure exceptional strength and quality. Additionally, hollow tube forgings offer a versatile and efficient solution for a wide range of construction and mechanical applications. Some key products benefits include reduced waste and enhanced structural integrity.
Why purchase Hollow Tube Forgings from qilu
Our custom-made hollow tube forgings provide a superior alternative to heavy wall steel pipe and mechanical tubing, offering higher quality.
They are a viable replacement for centrifugal castings, which frequently fail to meet the desired internal strength and integrity standards.
At Qilu, we have the expertise to forge hollows with unique configurations and geometries, including squares with a central hole or hollows with varying sizes on the outside diameter.

Ring Forgings

Our Ring Forgings can be forged into a wide range of configurations to meet your specific requirements. Whether you need flat, rectangular-cross section parts or tall, cylindrical shapes, each ring offers exceptional strength and toughness. Seamless ring forgings stand out as the superior choice when compared to castings, metal fabrications, or flame-cut plates, particularly for critical applications in industries like oil & gas, power generation, and aerospace.
Why purchase Rings Forgings from qilu
In terms of performance, ring forgings have no equal.
Their exceptional strength and ductility make them ideal for components that require resistance to torque, pressure, and fatigue.
At Qilu, we offer the most extensive capabilities of any ring forgings manufacturer globally, crafting each ring to order. Whether you need a single piece or high-volume orders, we have you covered.

Forged Shafts

Our products sets the bar high when it comes to mechanical performance. Thanks to our open-die forging process, we can control the grain flow throughout the product’s geometry, enhancing its characteristics and performance. Our forging capabilities deliver substantial cost and material savings in comparison to machined-bar step shafts.
Why purchase Forged Shafts from qilu
Our open-die forging process for shafts is essential for achieving the necessary high-mechanical properties while still preserving cost and material efficiency.
In terms of performance, ring forgings have no equal.
About
Qilu, as one of the leading forged metal manufacturers in China, specializes in the production of high quality forgings such as shaft forgings, ring forgings and disk forgings.
Contact Info
Address
Yanzhou,Economic,Zone,Jining,China
Email
Copyright © 2024 Qilu Steel Company